technical data>>
Speed of splicing single yarn 0.3-0.1 second/times, plied yarn 1.0-1.5 second/times
Rate of successfully splicing over 96% ( excluding faulty operation)
Length of splicing 20-25 mm adjustable
Diameter of splicing less than 1.3 times of that of original yarn
Air pressure 0.5-0.55 MPa for polyester fiber, 0.55-0.6£¼Mpa for pure cotton, 0.65-0.7Mpa for plied yarns, the air source must be clear without oil and water, stable in air pressure.
Air consumption 1-2 liter/times